ISO 12817:2013 specifies the test method to determine the open-hole compressive strength of laminated fibre-reinforced plastic composites. The laminate is intended to be a balanced and symmetrical lay-up or be otherwise homogeneous through the thickness. ISO 12817:2013 applies to all textile diameter fibre types (carbon, glass, aramids, etc.) and matrices (e.g. thermoset, thermoplastic) that meet its requirements.

ISO 12817:2013 includes three methods:

  • method 1 (short specimen with support fixture);
  • method 2 (short specimen without support fixture);
  • method 3 (long specimen with support fixture as in ASTM D 6484M-09, methods A and B).

Общая информация

  •  : В стадии разработки
    : Регистрация проекта международного стандарта (DIS) [40.00]
  •  : 2
  • ISO/TC 61/SC 13
    83.120 
  • RSS обновления

Жизненный цикл

Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)